Effect of Long Nozzle Casting with Shielding Argon Gas on Quality of Φ450 mm Round Billet of Wheel Steel

Wu Zongshuang1, Bao Yanping1, Liu Jianhua1, Chen Gang2, Gong Zhixiang2, Zhong Bin2   

  1. 1 School of Metallurgical and Ecological Engineering, University of Science and Technology, Beijing 100083;
    2 Maanshan Iron and Steel Co Ltd, Maanshan 243002
  • Received:2006-09-19 Online:2007-04-01 Published:2023-03-10

长水口氩封保护浇铸对车轮钢Φ450 mm 圆坯质量的影响

吴宗双1, 包 燕 平1, 刘 建 华1, 陈  刚2,  龚 志 翔2,钟 斌2   

  1. 1北京科技大学冶金与生态工程学院,北京100083;
    2马鞍山钢铁股份有限公司,马鞍山243002
  • 作者简介:吴宗双(1972-),男,工程师,1998年北京科技大学钢铁冶金专业毕业,炼钢连铸技术研究和产品开发。

Abstract: It is available to decrease gas content in steel by long nozzle casting with shielding argon gas. The examination results showed that in comparison without argon gas shielding casting the total oxygen content in φ450 mm round billet of wheel steel produced with shielding argon gas at Maanshan Steel decreased to 27.9×10-6, from original 49.3× 10-6, the total inclusion content in steel decreased to 14.8×10-6 from 29.7×10-6 the quality of cast billet obviously in- creased and the mechanical properties of wheel increased appreciably.

摘要: 钢包长水口采用氩封保护浇铸后,可有效降低钢中气体含量。检验结果表明,马钢车轮钢Φ450 mm圆坯的T[O]由未进行氩封保护浇铸时的49.3×10-6降到27.9×10-6,夹杂总量由29.7×10-6降至14.8×10-6,铸坯质量明显改善,车轮的力学性能显著提高。