Finite Element Analysis on Rolling Load Parameters of Hot Continuous Mandrel Rolling of T91 Steel Seamless Tube
Hong Huiping1, Zhao Zhiyi1 , Kang Yonglin1 , Yu Yong2, Zhou Xiaolan2, Pan Feng2
1 School of Materials Science and Engineering, University of Science and Technology, Beijing 100083 ;
2 Steel Tube Subcompany, Baoshan Iron and Steel, Shanghai 201900
Hong Huiping, Zhao Zhiyi , Kang Yonglin , Yu Yong, Zhou Xiaolan, Pan Feng. Finite Element Analysis on Rolling Load Parameters of Hot Continuous Mandrel Rolling of T91 Steel Seamless Tube[J]. Special Steel, 2006, 27(5): 3-5.
1王起江,邹凤鸣,张 瑞.宝钢T91高压锅炉管性能试验与研 究.宝钢技术,2003(4):46
2 Hong Huiping, Kang Yonglin, Feng Changtao. Three-dimensional Thermo-mechanical Coupled FEM Simulation for Hot Continuous Rolling of Large-diameter Mandrel Bar, Journal of Materials Science and Technology, 2003,19( Suppl) :228