Characteristics of Cooling of Nozzles for Secondary Cooling o 360mm×450mm Billet Concaster
Zhang Shuyan1,Zhu Miaoyong1,Chen Yong2,YangSubo3
1 School of Materials and Metallurgy,Northeastern University,Shenyang 110004;
2 Panzhihua Iron and Steel Research Institute,Panzhihua 617000;
3 Vanadium Recovery and Steelmaking Plant,Panzhihua Iron and Steel Co,Panzhihua 617062
Zhang Shuyan, Zhu Miaoyong, Chen Yong, Yang Subo. Characteristics of Cooling of Nozzles for Secondary Cooling o 360mm×450mm Billet Concaster[J]. Special Steel, 2006, 27(5): 24-26.