Simulation of Magneto-Crystalline Anisotropy Energy of Cold Rolled Non-Oriented Silicon Steel
Xu Xiangqi1, Jin Zili2
1 Department of Machinery, Tongling Institute, Tongling 244000 ;
2 School of Materials and Metallurgy, Inner Mongolia University of Science and Technology, Baotou 014010
Xu Xiangqi, Jin Zili. Simulation of Magneto-Crystalline Anisotropy Energy of Cold Rolled Non-Oriented Silicon Steel[J]. Special Steel, 2006, 27(5): 21-23.
1Arrott A S. The Past, the Present and Future of Soft Magnetic Materials, Magnetism and Magnetic Materials,2002,215 -216:6
2Hutchinson W B, Swift J G. Anisotropy in Some Soft Magnetic Materials. Texture, 1972( 1) : 117
3宛德福,马兴隆.磁性物理学.北京:电子科技大学出版社, 1994
4左 良,王沿东.广义矢量法预估多晶材料的磁晶各向异性. 金属学报,1990,26(4) :297
5 Bunge H J. Texture Analysis in Materials Science. Buttermorths, London ,1952:294