Abstract: The prospect of market of die steel products in China is systematically analyzed. The advance in plastics die steel, high cleanliness die steel, high isotropic die steel and die steel products,and the development of high performance die steel are presented in this article.
摘要: 系统地分析了我国模具钢产品的市场前景。介绍了国内外塑料模具钢、高纯净度模具钢、高等 向性模具钢以及模具钢品种的进展和新型高性能模具钢的开发。