ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2006, Vol. 27 ›› Issue (5): 40-42.

Previous Articles     Next Articles

Progress in Grades and Refining Technology of Ultra Purity Ferritic Stainless Steels

You Xiangmi,Jiang Zhouhua, Li Huabing   

  1. School of Materials and Metallurgy,Northeastern University,Shenyang 110004)
  • Received:2006-04-19 Online:2006-10-01 Published:2023-04-20

超纯铁素体不锈钢品种和精炼技术的进展

游香米, 姜周华 ,李花兵   

  1. 东北大学材料与冶金学院,沈阳110004

  • 作者简介:游香米(1981-),女,2003年东北大学毕业,在读博士生, 从事不锈钢冶炼工艺研究。

Abstract: The(C+N)content in ultra purity ferritic stainless steels is ≤150×10-⁶,its corrosion resistance, weldability and toughness are obviously higher than that of common ferritic stainless steels. The grade,chemical com- position and properties of new developed ultra purity fernitic stainless steels including modified 409,429 and modi- fied,444 and modified steels are presented; and by using 3- step steel making process to produce 18Cr ultra purity ferritic stainless steels, with SS-VOD refining,the(carbon + nitrogen)content in steel-[C+N] is≤70×10-6, with VOD-PB refining,[C+N] is 80×10-6,and with VCR refining,[C+N] is(80~100)×10-⁶.

摘要: 超纯铁素体不锈钢中(C+N)含量≤150×10- °,其耐蚀性、焊接性能、韧性等显著高于普通铁素  体不锈钢。介绍了新开发的409改进型、429及改进型、444及改进型超纯铁素体不锈钢的钢种、成分和性能; 采用三步法工艺冶炼18Cr超纯铁素体不锈钢,用SS-VOD 精炼时,钢中[C+N]≤70×10-⁶ ;VOD-PB 精炼时, [C+N] 为80×10-⁶ ;VCR 精炼时,[C+N] 为(80~100)×10-⁶。