Analysis on Quality of Corrosion-Resisting Mirror Plastic Die Steel 4Cr13(1.2083)

Guan Yingchun1,Tang Guoyi1,Ye Qiang2   

  1. 1 Institute of Advanced Materials,Craduate School of Shenzhen,Tsinghua University,Shenzhen 518055;
    2 Shenzhen Yuding Die Steel Co Ltd,Shenzhen 518107
  • Received:2006-04-24 Online:2006-10-01 Published:2023-04-21

耐蚀镜面塑料模具钢4Cr13(1.2083)质量的分析

管迎春¹, 唐国翌¹, 叶 强²   

  1. 1清华大学深圳研究生院新材料研究所,深圳518055;
    2深圳裕鼎模具钢有限公司,深圳518107
  • 作者简介:管迎春(1983-),女,硕士研究生,从事模具材料及加工新 技术研究。

Abstract: Metallurgical quality and mirror polishing performance of domestic wide used 5 kinds of ESR high quality corrosion-resisting mirror plastic die steel 4Cr13(DIN 1.2083)-0.37~0.57C,12.59~13.67Cr produced at home and abroad are analyzed comprehensively. Examination results indicated that the ESR steels have excellent mirror polishing performance,as the range of HRC hardness value of samples was ≤1.5,the steels have nice mirror polishing performance and as there were multi-phase titanium nitride inclusions in steel,they obviously influenced the mirror polishing performance of steel.

摘要: 综合分析了国内普遍使用的成分(%)为0.37~0.57C、12.59~13.67Cr的5种国内外钢厂生产 的电渣重熔4Cr13(DIN 1.2083)高级耐蚀镜面塑料模具钢的冶金质量和抛光性能。测试结果表明,该钢经电 渣重熔后具有较好的抛光性能,当试样的HRC 硬度值的极差≤1.5时,钢具有较好的抛光性能;当钢中存在 复相氮化钛夹杂时,显著影响该钢的抛光性能。