Practice of Boron Microalloying Process of SPHC Steel for Cold Rolling

Xu Zhirong1,Yan Huicheng2,Qiu Shengtao2,Liu Jiaqi2,Liu Jianhua1,Kong Qingfu1, Bai Lianchen1, Chen Libin1#br#   

  1. 1 Tangshan Steel Co Ltd,Tangshan 063016;
    2 National Engineering Research Center of Continuous Casting Technology,Central Iron and Steel Research Institute,Beijing 100081
  • Received:2006-03-31 Online:2006-10-01 Published:2023-04-21

冷轧用 SPHC 钢硼微合金化工艺实践

徐志荣¹ 颜慧成² 仇圣桃² 刘家琪² 刘建华¹ 孔庆福¹ 白连臣¹ 陈礼斌¹   

  1. 1唐山钢铁股份有限责任公司,唐山063016;
    2钢铁研究总院国家连铸工程中心,北京100081
  • 作者简介:徐志荣(1962-),男,工学硕士,厂长,从事钢铁冶金领域 研究与生产组织工作。

Abstract: The boron microalloying process of SPHC steel(≤0.07%C,≤0.05%Si)for cold rolling pro- duced by 160 LD- 160 t LF-FTSR(Flexible Thin Slab Rolling)flow sheet has been developed at Tangshan Steel, and with controlling Al content in steel(average 0.038%)and Si content(average 0.038%)during LF refining, the boron content in steel after LF refining was 0.0030%~0.0040%(average content 0.0035%),and the boron yield was up to 64%.

摘要: 开发了唐钢160 t LD- 160 t LF-FTSR(Flexible Thin Slab Rolling) 流程生产冷轧用SPHC 钢(≤ 0.07%C,≤0.05%Si) 硼微合金化工艺,通过在精炼过程控制钢中Al含量(平均0.038%)和 Si含量(平均 0.038%),使LF 精炼后钢中的硼含量为0.0030%~0.0040%(平均含量0.0035%),硼的收得率达64%。