Abstract: It is basic condition for production of cleanliness to control Are furnace[P][S], total amount of [Pb] and [Zn].To prevent rephosphorization and slag free tapping are key operations to get low [P][S] molten steel of arc furnace. AS melting down the [Pb] exceeds standard limit, first stop carbon injection operation and increase blown oxygen amount and angle to decrease [C] less than 0. 10%, with molten steel stirring and heating for 2~6 min to promote [Pb] which deposits at bottom, solubilized in steel, oxidized and trapped by slag, then inject foaming agent carbon powder to reduce Pb oxide to Pb which evaporates and exhausts. The de-[Pb] ratio was 19.0%~46.4%.T he de-[Zn] operation is similar to that of de-[Pb].
摘要: 控制电弧炉[P][S]含量和[Pb][Zn]总量,为生产洁净钢创造了基本条件,防止炉渣回磷和无渣出钢操作是获得低[P][S]电弧炉钢水的关键操作。应控制炉料中[Pb][Zn]含量,当熔清时,[Pb]等成分超出标准要求的情况下,首先停止喷碳操作,增大吹氧强度和角度,将[C]降至0.10%以下,钢水经搅拌和升温,促使沉降在炉底[Pb]通过钢水的溶解、氧化被炉渣捕集,2~6min后,喷入发泡剂碳粉,使Pb氧化物还原成Pb蒸发排出,脱[Pb]率为19.0%~46.4%。脱[Zn]操作与脱[Pb]相同。
Wang Xincheng , Yu Haiming. Operation Practice of De- [P][S] and [Pb][Zn] in Arc Furnace[J]. Special Steel, 2005, 26(4): 44-45.
王新成, 俞海明. 电弧炉脱[S][P]和[Pb][Zn] 的操作实践[J]. 特殊钢, 2005, 26(4): 44-45.
0 / / Recommend
Add to citation manager EndNote|Ris|BibTeX
URL: https://www.specialsteeljournal.com/EN/
https://www.specialsteeljournal.com/EN/Y2005/V26/I4/44