Research and Production on Medium and Heavy Plate of HQ590DB Ultra-Low Carbon Bainitic Steel

Zhao Zhiping ,Kang Yonglin,Cong Jingong ,Zhang Xiaogang   

  1. University of Science and Technology, Beijing 100083
    Anshan New Rolling Steel Co Ltd, Anshan 114021)
  • Received:2005-07-14 Online:2005-02-01 Published:2023-05-24

HQ590DB超低碳贝氏体钢中厚板的研制

赵志平,康永林,丛津功,张晓刚   

  1. 北京科技大学材料学院,北京100083 ,
    北京科技大学材料科学与工程学院,北京100083 ,
    鞍山新轧钢股份公司,鞍山114021 ,
    鞍山新轧钢股份公司,鞍山114021
  • 作者简介:赵志平,男,39岁,高级工程师,在职博士研究生。从事轧钢工艺技术的调整和控制及生产技术管理。

Abstract: The 30~40 mm medium plate of HQ590DB ultra-low carbon bainitic steel - 0.05C- 1.5Mn-0.04Nb- 0.02Ti-≤0.0002B has been pilot-produced by 180 t converter- RH - LF (Ca treated)- concasting slab:230(300)mmx1650mm×6000 mm-4300 mill controlled rolling and cooling process. [H] in concasting slab was 1.7×10-⁶,[O] 21 ×10~⁶ and[N]29×10-6.With controlled finishing rolling temperature between 800 and 850 ℃ and cooling temperature between 590 and 630 ℃, the structure of ferrite + lath bainite was obtained, the tensile strength σb of plate was 650~690 MPa, yield strength σ0.2 490~590 MPa, elongation δ5 20%, and the plate has excellent formability.

摘要: 采用 18 0t转炉 RH LF(Ca处理 ) 连铸坯 (mm) :2 30 (30 0 )× 16 5 0× 6 0 0 0 4 30 0轧机控轧控冷工艺试制了HQ5 90DB超低碳贝氏体钢 (% ) :0 0 5C ,1 5Mn ,0 0 4Nb ,0 0 2Ti,≤ 0 0 0 0 2B的 30~ 4 0mm中板。连铸坯的 [H]1 7× 10-6 ,[O]2 1× 10 -6,[N]2 9× 10-6 。终轧温度 80 0~ 85 0℃ ,控制终冷温度 5 90~ 6 30℃ ,获得铁素体+板条状贝氏体组织 ,钢板抗拉强度σb6 5 0~ 6 90MPa ,屈服强度σ0.2 4 90~ 5 90MPa ,延伸率δ2 0 % ,并具有良好的成形性能。