[1] |
Zhao Qian, Liu Haixiao, Li Ming, Wang Bing, Li Ba, Jia Shujun, Liu Qingyou.
Study on the Effects of Partial Pressure on X52M Pipeline Hydrogen Embrittlement Properties in High-Pressure Hydrogen Environments
[J]. Special Steel, 2025, 46(3): 117-124.
|
[2] |
Liu Junkai, Yu Yipeng, Shen Yaqiu, Wang Jing, Luo Xi, Zhang Jiansheng.
Mechanical Properties of Ni-Cr-Al Alloy Cold Drawn Bar
[J]. Special Steel, 2025, 46(3): 34-37.
|
[3] |
Liu Wenxue, Liu Guanghui, Li Linsen, Fei Sanlin, XuYong, XieWei, Xu Guangpeng, Ni Yanhong.
Influencing Factors and Process Control of Vacuum Consumable Remelting Arc Stability
[J]. Special Steel, 2025, 46(3): 12-17.
|
[4] |
Hou Shiyao, Zhang Yang, Yang Dongou, Zhao Yang, Chen Liqing.
Ultra-High Strength 50SiMnCr Spring Flat Steel and its Continuous Cooling Transformation Behavior
[J]. Special Steel, 2025, 46(2): 98-102.
|
[5] |
Wang Zhanzhong, Zhang Yue, Li Xu, Peng Feng, Liu Dan, Guo Shibei, Liu Yueyun.
Production Process Practice of 42CrMoM Steel for 12.9 Grade High Strength Wind Power Fasteners
[J]. Special Steel, 2025, 46(2): 38-42.
|
[6] |
Chen Dengguo, Lv Jiping, Wan Yong, Dong Fujun, Cao Ruihong, Sun Lefei.
Inclusion Evolution and Calcium Treatment Optimization of 9Ni Steel
[J]. Special Steel, 2025, 46(1): 66-74.
|
[7] |
Peng Feng, Li Xu, Li Bopeng, Zhang Yue, Wang Zhanzhong, Guo Shibei.
Development of 10.9 Grade 32CrB4 Quenched and Tempered Round Steel for Fasteners
[J]. Special Steel, 2024, 45(6): 8-11.
|
[8] |
Zhao Jiawei, Tian Jialong, Yang Ping, Zhan Dongping, Jiang Zhouhua.
Effect of Dual-aging Process on Microstructure and Properties of Co-precipitation Hardening Ultra-high Strength Steel
[J]. Special Steel, 2024, 45(6): 88-94.
|
[9] |
Zhao Bo, Wang Shanbao, Xie Degang, Yuan Qin, Ai Fangfang, Wang Xixiang, Guo Jinmei.
Microstructure and Properties of Seamless Steel Pipe Gr.6 after Rolling and Normalizing
[J]. Special Steel, 2024, 45(6): 102-107.
|
[10] |
Tang Yuanshou, Zhang Shiqing, Li Fang, He Qinsheng, Zhao Zhen, Wang Hong, Zou Xingzheng, Wang Jianqiao, Huang Yali.
Effect of Quenching Temperature on Mechanical Properties of M6C Reinforced 2 200 MPa Ultra-high Strength Steel
[J]. Special Steel, 2024, 45(5): 108-112.
|
[11] |
Wang Shaobing, Sun Wenqiang, Wang Man, Zhou Zhu, Liu Zhengdong, Zhong Qiang.
The Effect of Nb on Microstructure and Properties of GH4169 Alloy Pipe
[J]. Special Steel, 2024, 45(5): 34-39.
|
[12] |
Wang Shucai, Guo Jing, Wu Zhilong, Han Kui, Zhao Yue, Chen Xiuqiang.
Low-cost Non-vacuum Induction Furnace Smelting of High Molybdenum Content of Nickel-base Alloy
[J]. Special Steel, 2024, 45(5): 72-75.
|
[13] |
Li Qing.
Effect of Solid Solution Temperature on Microstructure and Tensile Properties of GH4163 Alloy
[J]. Special Steel, 2024, 45(5): 97-101.
|
[14] |
Yang Zhihao, Wang Linlin, Liang Tian, Jia Dongxiao, Ma Yingche, Wang Ping.
Effect of Rare Earth Gd on Thermal Deformation Behavior of Ni-Cr-Mo Alloys
[J]. Special Steel, 2024, 45(5): 8-18.
|
[15] |
Li Yang, Zhao Guangdi, Zang Ximin, Jiang Haoyuan, Wang Zhaoyu.
Effect of Boron on the Microstructure and Strength-Toughness of Fe-Cr-B-C Alloy after Heat Treatment
[J]. Special Steel, 2024, 45(5): 25-33.
|