ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2020, Vol. 41 ›› Issue (1): 24-27.

Special Issue: 铁素体不锈钢

Previous Articles     Next Articles

AOD Nitrogen Control Pratice of of Low Carbon 400 Series Ferritic Stainless Steel at Xingtai Iron and Steel

Li Guangbin1,2, Zhao Yingkai1, Wu Guanghai1, Yang Qiangqiang1 ,MuYongwei 1, Guo Zhibin1   

  1. 1 Stainless Steel Company,Xingtai Iron and Steel Co Ltd,Xingtai 054027 ;
    2 Hebei Wire and Cable Engineering Technology Research Center,Xingtai 054027
  • Received:2019-06-22 Online:2020-02-01 Published:2022-04-19

邢钢低碳400系铁素体不锈钢AOD控氮工艺实践

李广斌1,2,  赵迎凯1, 吴广海1, 杨强强1,木永卫1, 郭志彬1   

  1. 1邢台钢铁有限责任公司不锈钢公司,邢台054027 ;
    2河北省线材工程技术研究中心,邢台054027
  • 作者简介:李广斌(1985-),男,工程师,2010年内蒙古工业大学(本 科)毕业,不锈钢产品生产研发及管理。

Abstract:  Nitrogen can deteriorate intergranular corrosion, low temperature impact toughness, notch sensitivity and soldering properties of low carbon 400 series stainless steel. Therefore, reducing the nitrogen content under the premise of low consumption and high efficiency has become an important issue in AOD smelting. Combined the production test, by exploring the application of regression analysis in the control of argon-denitrification process and combined with the thermodynamic calculation of denitrification to analyze the production data of AOD, it is determined by the fitting equation that the switching point of nitrogen to argon is at blowing nitrogen 450 m3 ,the normal blowing argon amount of 410S stainless steel in AOD is controlled at 1550m3, and the blowing argon amount of low carbon 430 stainless steel in AOD is generally con¬trolled at 2050mto get controlled [N] below 0.0090% and reduce of argon consumption.

Key words: Low Carbon 400 Series Stainless Steel, AOD, Nitrogen Argon Switching Point ,

摘要: 在低碳400系不锈钢中,氮能恶化晶间腐蚀、低温冲击韧性、缺口敏感性和焊接等性能。因此,在低耗、高效前提下降低其氮含量成为AOD冶炼中的重要课题。结合生产试验,通过探讨回归分析法在其吹氩脱氮工艺控制中的应用,结合脱氮的热力学计算对AOD生产实践数据的分析,由拟合方程确定的AOD冶炼410S不锈钢和低碳430不锈钢时氮氩切换点为吹氮450m3时切换氩气,410S不锈钢正常冶炼时一般吹氩量控制在1550m3,低碳430不锈钢AOD吹氩量一般控制在2050m3时可以将AOD终点氮含量控制在0.009 0%以下,并降低氩气消耗。

关键词: 低碳400系不锈钢, AOD, 氮氩切换点