[1] |
Yuan lin, Hu Xiaoqiang, Liu Yang, Li Dianzhong, Xie Jing, Chen Wei.
Comparative Analysis of 3%Cr Roller Steel by Rare Earth Refining and Electroslag Remelting
[J]. Special Steel, 2024, 45(5): 1-7.
|
[2] |
Liu Ye, Gui Yulin, Yin Qing, Wu Xiaolin, Miao Xinde.
Research on Ultra-high Rotary Bending Fatigue Strength of Flexible Bearing Steels for Robot Harmonic Speed Reducer
[J]. Special Steel, 2024, 45(3): 105-113.
|
[3] |
Wang Weimin, Qi Haiquan , Han Xiangnan, Sui Wenjie, Liu Anqi, Guo Chuncheng, Da Zhongzhong, Wan Yu, Li Wentong.
Effect of Mo Microalloying on High Temperature Mechanical Properties and Microstructure of 82B Steel
[J]. Special Steel, 2024, 45(2): 79-85.
|
[4] |
Yu Wenchao, Xie Dirong, Shi Jie, Wang Maoqiu.
Influence of Sulfur Content on Inclusion and Fatigue Properties of 18CrNiMo7-6 Gear Steels
[J]. Special Steel, 2024, 45(1): 111-116.
|
[5] |
WANG Shaobing, SUN Wenqiang, WANG Man, ZHOU Zhu, ZHANG Yanyan.
Application of Gleeble Thermal Simulation for Hot Plasticity of S32750 Austenito-Ferrite Duplex Steel
[J]. Special Steel, 2022, 43(4): 5-9.
|
[6] |
TU Xingkuang, XU Jianfei, ZHOU Miao, SU Zhenwei, LIN Jun, WAN Wenhua.
Study on Cleanliness Controlling of Liquid of Low Carbon Al-killed 0.20 C Steel
[J]. Special Steel, 2022, 43(3): 35-38.
|
[7] |
TU Xingkuang, XU Jianfei, YANG Chengwei, SU Zhenwei, HUANG Yunfei.
Effect of BOF-RH-CC and BOF-LF-CC Process on Cleanness of Cold Heading Steel ML08Al
[J]. Special Steel, 2022, 43(3): 56-59.
|
[8] |
Sui Wenjie, Li Tianran, Han Xiangnan, Liu Yang, Qing Xiangzhi , Qi Haiquan.
Effect of Mo Microalloying on Structure and Mechanical Properties of 82B High Carbon Steel for Architecture
[J]. Special Steel, 2022, 43(2): 64-68.
|
[9] |
Li Guiying, Li Maimai.
Investigation of Drawing Fracture Cause of C82D2 Steel Wire for Steel Cord for Tyre and Process Improvement
[J]. Special Steel, 2021, 42(4): 30-34.
|
[10] |
Cheng Hanwen, Zhao Guochang, Lin Mingxin, Xie dong, Shi Li , Xiao Xiongfeng.
Effect of Heat Treatment Process on Structure and Properties of SA-738Gr. B Steel Plate for Nuclear Power Station
[J]. Special Steel, 2021, 42(2): 56-59.
|
[11] |
Fei Shangcai , Jiang Xiaoxia, Gou Ningnian , Xu Nan.
A Study on Non-Metallic Inclusion in DQ Deep-Drawing Low Carbon Steel Casting Slab Produced by CSP Process
[J]. Special Steel, 2020, 41(4): 37-39.
|
[12] |
Lu Naishuang, Liang Na , Huang Tao.
Study on Control Technology of Non-metallic Inclusions in 25MnBM Steel for Track Plate
[J]. Special Steel, 2020, 41(3): 25-27.
|
[13] |
Xie Zhibin , Shao Qingli, Zhang Guoping, Wang Kai, He Ning.
Research on Quality of high Speed Steel M35 Bearing Sulfur Remelting by Acid Slag
[J]. Special Steel, 2019, 40(1): 27-30.
|
[14] |
Lin Yuan , Zhang Wenkang.
Effect of Annealing Temperature and Recrystallized Grain Rate on Properties of 0.50 mm Cold-Rolled Sheet of 0.58Si Non-Oriented Silicon Steel
[J]. Special Steel, 2017, 38(4): 53-56.
|
[15] |
Ye Fanxin , Feng Wenfu , Guo Zhibin , Wang Xiaoliang , Cao Hongbo , Wu Guanghai.
Process Practice of Steelmaking of Ultra Low [C+N] Stainless Steel 0Cr13 for Cleaning Ball by 60t AOD-LF-CCM Flowsheet
[J]. Special Steel, 2017, 38(2): 23-25.
|