ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2024, Vol. 45 ›› Issue (5): 119-122.DOI: 10.20057/j.1003-8620.2023-00002

Previous Articles     Next Articles

Effect of Thread Processing Sequence on Room Temperature Fatigue Performance of A286 Fasteners

Kong Xiangwei , Hou Meiling , Bai Yun , Zhang Jianfeng   

  1. Special Steel Institute, Jiangyin Xingcheng Special Steel works Co.,Ltd., Jiangyin 214400, China
  • Received:2023-01-06 Online:2024-09-30 Published:2024-10-01

螺纹加工顺序对A286紧固件室温疲劳性能的影响

孔祥伟,侯美伶,白 云,张剑锋   

  1. 江阴兴澄特种钢铁有限公司特钢研究院,江阴 214400
  • 作者简介:孔祥伟(1988—),男,工程师;E-mail:kongxiangwei@citicsteel.com

Abstract: The high frequency tensile fatigue test of heat-resistant fasteners of A286 alloy with different thread processing sequences was carried out by means of axial fatigue testing machine, metallographic microscope, microhardness tester and scanning electron microscope, and the metallographic of fatigue fracture and thread was analysed . The results show that machining thread after 720 ℃-12 h aging is beneficial to improve the stability of fatigue performance of fasteners, and has a slight effect on the median fatigue strength, but has no effect on the fatigue fracture mode. A large number of twins are formed on the surface of machined threads before aging, and the reinforced phase precipitates out at the twin boundary with large size particles during aging. Because the hardness of fasteners threaded before aging fluctuates greatly, it may also be the cause of the fluctuation of fatigue performance.

Key words: Heat-resistant fastener, High temperature alloy, Thread, Fatigue Performance

摘要: 采用轴向疲劳试验机、金相显微镜、显微硬度计和扫描电镜等方法,通过对不同螺纹加工顺序的A286合金耐热紧固件进行高频拉-拉疲劳测试,并对疲劳断口和螺纹的金相进行分析。结果表明,在经过720 ℃-12 h时效后加工螺纹,有利于提高紧固件疲劳性能的稳定性,对疲劳中值强度略有影响,对疲劳断裂方式无影响。时效前加工螺纹,会在紧固件表面形成大量的孪晶,时效过程中强化相会在孪晶界以大尺寸颗粒析出。时效前加工螺纹的紧固件其螺纹根部硬度值波动大,可能是造成疲劳性能波动大的原因。

关键词: 耐热紧固件;高温合金;螺纹;疲劳性能