ISSN:1003-8620
CN:42-1243/TF
Governed by: CITIC Pacific Special Steel Group Co., LTD
Sponsored by: Daye Special Steel Co., LTD.
Special Steel ›› 2024, Vol. 45 ›› Issue (3): 1-4.DOI: 10.20057/j.1003-8620.2023-00011
Next Articles
Li Bopeng1,2, Tao Shijun 1, Zhang Jianfeng1, Liu Yueyun1,2, Lu Zhujun1,2, Lv Wenjun1
Received:
Online:
Published:
李博鹏1,2 ,陶士君1 ,张剑锋 1,刘月云 1,2,陆竹君1,2 ,吕文俊1
Abstract: Based on the current quality situation of ESR bearing steel for passenger railway and wagons in China, the grade 8620 steel bars with diameters between 60 mm and 120 mm are produced with the process as follows:70 t EAF(HotMetal+Scrap)→LF→RH→3 t steel ingot→soaking pit →1350+750/650 rolling mill, whose chemical composition are (%):0. 18-0. 22 C,0. 15-0. 30 Si,0. 75-0. 95 Mn,0. 45-0. 65 Cr,0. 45-0. 70 Ni,0. 15-0. 25 Mo,≤0. 020 P,≤0. 015 S, 0. 020-0. 050 Al. By taking technological measures such as steel and slag retention operation,slag formation and alloy ad⁃ dition during tapping, vacuum holding time ≥25 min and soft argon blowing, superheat control, full process Argon protec⁃ tion casting and automatic pouring as well as controlling cooling after rolling etc, to keep 8620 steel bars conform to all technical specification requirements, especially, macro-inclusions of finished bars less than 10 mm/dm³, grain size class 8-8. 5, and the density being 7. 854 g/cm³.
Key words: 3 t Steel Ingot; Grade 8620 Steel; Automatic Ingot Casting, Macro-inclusion; Density
摘要: 针对中国铁路客车和货车轴箱轴承用钢主要使用电渣钢的现状,采用铁水+废钢→70 t 电弧炉→LF→RH→ 3 t 钢锭→均热坑→1350+750/650 轧机轧制的流程生产规格 ϕ60~120 mm 8620 钢(/%:0. 18~0. 22 C,0. 15~0. 30 Si,0. 75~0. 95 Mn,0. 45~0. 65 Cr,0. 45~0. 70 Ni,0. 15~0. 25 Mo,≤0. 020 P,≤0. 015 S,0. 020~0. 050 Al)。通过 控制出钢留钢留渣、炉后造渣和合金化,真空处理时间≥25 min,氩气弱搅拌,控制钢水过热度,全过程Ar气保护,模 铸自动浇注,轧制后控制冷却等工艺措施,生产的产品宏观夹杂物检测含量≤10 mm/dm3 ,晶粒度8~8. 5级,密度达 到7. 854 g/cm³,钢材各项指标满足标准要求。
关键词: 3 t钢锭, 8620钢, 模铸自动浇注, 宏观夹杂物, 密度
CLC Number:
TF119
Li Bopeng , Tao Shijun, Zhang Jianfeng, Liu Yueyun, Lu Zhujun, Lv Wenjun. Development of Rolled Steel Products from 3 t Ingot of Grade 8620 for Railway Axle Box Bearings[J]. Special Steel, 2024, 45(3): 1-4.
李博鹏, 陶士君, 张剑锋, 刘月云, 陆竹君, 吕文俊. 铁路轴箱轴承用8620钢3 t钢锭轧制产品研发[J]. 特殊钢, 2024, 45(3): 1-4.