Inclusion Evolution and Calcium Treatment Optimization of 9Ni Steel

Chen Dengguo1, Lv Jiping1, Wan Yong2, Dong Fujun1, Cao Ruihong1, Sun Lefei1   

  1. 1 Xinyu Iron and Steel Co., Ltd., Xinyu 338001,China;
    2 School of Metallurgical Engineering, Anhui University of Technology, Ma’anshan 243032, China
  • Received:2024-07-26 Online:2025-02-01 Published:2025-01-16

9Ni钢夹杂物演变及钙处理工艺优化

陈登国1, 吕继平1, 万勇2, 董富军1, 操瑞宏1, 孙乐飞1   

  1. 1 新余钢铁股份有限公司,新余 338001;
    2 安徽工业大学冶金工程学院,马鞍山 243032
  • 通讯作者: 万勇
  • 作者简介:陈登国(1981—),男,高级工程师
  • 基金资助:
    赣鄱俊才支持计划—主要学科学术和技术带头人培养项目

Abstract: By means of industrial test and Aspex automatic inclusion analysis techonogy, the evolution law of [T.O], [N] content, microinclusions quantity, size and type of 9Ni steel in LF→RH→CC steelmaking process were systematically studied. The formation mechanism of calcium-aluminate and CaS inclusions under calcium treatment conditions was investigated by Factsage software. The results show that the content of [T.O] and [N] in 9Ni steel increases simultaneously in the process interval from LF first power supply→LF second power supply and RH soft blowing argon gas for 20 min→rolling, indicating that there is secondary oxidation in the molten steel in these two process intervals. The inclusions in 9Ni steel are mainly CaO-Al2O3-MgO and CaO-Al2O3-CaS complex inclusions, and the size is mainly between 2 μm-5 μm. When the calcium line is reduced from 200 m to 100 m, the density of 2 μm-5 μm inclusions in 9Ni steel rolled material is significantly reduced, and basically no inclusions containing CaS components are found, and the grades of DT and DS inclusions are reduced from 1.0 and 1.5 grades to 0.5 and 0.5 grades, respectively. The Aspex statistical results of the density, size and average composition of composite inclusions in 9Ni steel rolled sheets with 200 m and 100 m calcium line are in good agreement with the inclusion rating results and Factsage calculation results.

Key words:  , 9Ni Steel; Inclusion Transformation; Calcium Treatment; CaS; Factsage Calculation

摘要: 通过工业试验和Aspex全自动夹杂物分析技术,对9Ni钢在LF→RH→CC炼钢过程[T.O]、[N]含量、显微夹杂物数量、尺寸及类型的演变规律进行了系统研究,并结合Factsage软件探究了钙处理条件下钙铝酸盐和CaS夹杂的形成机理。结果表明,在LF第一次送电结束→LF第二次送电结束和RH软吹氩气20 min→轧材这两段工艺区间,9Ni钢中[T.O]、[N]含量均同时升高,表明在这两段工艺区间钢液存在二次氧化。9Ni钢轧材中夹杂物类型以CaO-Al2O3-MgO和CaO-Al2O3-CaS复合夹杂为主,尺寸主要位于2~5 μm。当钙线量从200 m降至100 m,9Ni钢轧材中2~5 μm的夹杂物密度明显减小,基本未发现含CaS组分的夹杂物,其D类细系、DS类夹杂物评级分别从1.0、1.5级降至0.5、0.5级。喂钙线200、100 m的9Ni钢轧材中复合夹杂物的密度、大小和平均成分的Aspex统计结果与其夹杂物评级结果和Factsage计算结果均具有较好的一致性。

关键词: 9Ni钢, 夹杂物演变, 钙处理, CaS, Factsage计算