ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Study on Deoxidation, Desulfurization and Inclusion Control of SiCaBa Alloy on Spring Steel 55SiCr
Liu Jinwen, Tie Zhanpeng, Guo Luzhao, Zhang Shuo, Zhang Jiaquan , Tang Haiyan
Special Steel . 2020, (3): 20 -24 .