Effect of Cold Rolling Reduction on Texture and Formability of Ultra-Clean Ferrite Stainless Steel Cr22Mo
Zhou Jie, Zhao Zhenduo, Lian Xiaojie, Fan Guangwei, Wang Ldxin, Zhang Jingjing, Cheng Shengwei,
Special Steel . 2018, (5): 70 -74 .