Process Practice of Control Oxygen Content in Bearing Steel GCr15 Produce by 80t BOF-LF-VD-CC Flowsheet
Liu Fayou , Wang Guocheng , Sun Changyu , Zhao Changming , Wang Qi , Mao Fulai
Special Steel . 2016, (5): 36 -36 .