Process Practice of Control Oxygen Content in Bearing Steel GCr15 Produce by 80t BOF-LF-VD-CC Flowsheet

Liu Fayou1,2, Wang Guocheng1, Sun Changyu1, Zhao Changming1 , Wang Qi1 , Mao Fulai2   

  1. 1. School of Materials and Metallurgy, Liaoning University of Science and Technology, Anshan 114051 ;
    2. Shandong Shouguang Juneng Special Steel Co Ltd, Weifang 262711 ;
  • Received:2016-05-04 Online:2016-10-01 Published:2022-07-30
  • Supported by:
    辽宁省自然科学基金项目资助(2015020181)

80t BOF-LF-VD-CC流程生产GCr15轴承钢控氧的工艺实践

刘发友1,2,王国承1,孙长余1,赵昌明1,汪琦1,毛福来2   

  1. 1. 辽宁科技大学材料与冶金学院,鞍山 114051 ;
    2. 山东寿光巨能特钢有限责任公司,潍坊 262711;
  • 作者简介:刘发友(1970-),男,博士生,山东大学(本科)毕业,轴承钢冶炼研究。

Abstract: The effect of BOF end [C] on end [O] and the effect of LF refining slag ( FeO + MnO) and [Als] in steel on liquid [O] and finished products T[O] are analyzed. With using the process measures including controlling BOF end [C] 0.12%~0.15% and amount of slagging out <0.10% , controlling [Als] 0.015%~0.025% in LF refining, using high basicity tundish shielding agent and special bearing steel GCr15 casting powder, in stable process control condition the T[O] in steel ≤10 X 10-6 and the average T[O] is 6. 62 x 10-6

Key words: 80t BOF-LF-VD-CC Flowsheet, Bearing Steel GCr15, T[O], end [C], [Als], Refining Slag, Shielding Casting

摘要: 分析了BOF终点[C]对终点[O]的影响,LF精炼渣(FeO+MnO)和[Als]对钢水[O]和钢材T[O]的影响。通过控制BOF终点[C]0.12%~0.15%,下渣量<0.10%,LF精炼控制[Als]0.015%~0.025%,采用高碱度中间包覆盖剂和专用GCr15钢连铸保护渣等工艺措施,在稳定工艺控制的条件下,可使钢中T[O]≤10×10-6,平均T[O]为6.62×10-6

关键词: 80t BOF-LF-VD-CC流程, GCr15轴承钢, T[O], 终点[C], [Als], 精炼渣, 保护浇铸