Effect of Temperature on Diffusion of Si in 1.6Si Non-Oriented Silicon Steel during Molten Salt Electro-Deposit Process
Li Hui, Liang Jinglong, Zhao Xiaoping, Li Yungang, Zhang Fenping
Special Steel . 2014, (6): 12 -14 .