Practice on First Deslagging Process of Double Slag Dephosphorization in 120 t Top and Bottom Combined Blown Converter
Wu He, Li Jin, Zhou Chaogang, Cai Kesen, Wu Guoping, Cao Yuliang
Special Steel . 2013, (6): 30 -32 .