Evolution of Inclusions in Stainless Steel 304 during Dephosphorized Hot Metal-110 t AOD-LF-CC-Hot Rolling Process
Chen Chao, Hou Haibin , Cheng Guoguang , Pan Jixiang, Li Yan and Pan Wei
Special Steel . 2013, (1): 41 -44 .