Hydraulic Simulation of Optimization of Flow Control Devices for a Tundish of Eight-Strand Continuous Casting
Wang Hongbin, Tang Haiyan, Li Jingshe , Bai Liguo
Special Steel . 2012, (3): 18 -21 .