Process Practice of Arc Caster Producing φ1200 mm S355NL/Q355NE Steel Continuous Casting Round Bloom
Zhou Kaiming, Dong Juan
Special Steel . 2023, (1): 10 -14 .  DOI: 10.20057/j.1003-8620.2022-00096