ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2023, Vol. 44 ›› Issue (1): 10-14.DOI: 10.20057/j.1003-8620.2022-00096

Special Issue: 连铸工艺

Previous Articles     Next Articles

Process Practice of Arc Caster Producing φ1200 mm S355NL/Q355NE Steel Continuous Casting Round Bloom

Zhou Kaiming,Dong Juan   

  1. Jiangyin Xingcheng Special Steel Works Co.,Ltd.,Jiangyin 214429
  • Received:2022-07-16 Online:2023-02-01 Published:2023-01-20

弧形连铸机生产S355NL/Q355NE钢Φ1 200 mm连铸圆坯的工艺实践

周开明, 董娟   

  1. 江阴兴澄特种钢铁有限公司研究院棒材研究所
  • 作者简介:周开明(1979-) ,男,硕士,工程师;

Abstract: Φ1200 mmS355NL/Q355NE steel (Ceq0.38-0.41) continuous casting round bloom is manufactured by 100 t KR-BOF-LF-RH-R18M continuous casting process. Full protective casting, precise cooling process, three-stage electro- magnetic stirring, slow cooling process and other technical measures are adopted. The superheat is controlled at 1545 ℃, the drawing speed is 0.14-0.20 m/min, the electromagnetic stirring is 300 A/2 Hz, the secondary cooling water ratio is 0.20 L/kg, the slow cooling time into the pit is ≥72 h, and the pit exit temperature is ≤300 ℃. The results show that [0]≤0.0018%,[H]≤0.00008%; the central porosity of cast bloom≤1.5  rating, the central crack≤1.5 rating, the shrinkage cavity ≤0.5 rating, and the carbon content range of the whole section≤0.07%. Chemical composition, macrostruce, surface quality all meets the standard requirements. After the round bloom is forged into wind turbine flanges with wall thickness of 450-550 mm by customer, the test results of inclusions, mechanical properties, internal flaw detection and other quality indexes are satisfactory, which fully meet the technical specifications and user requirements.

Key words: Φ1 200 mm, Large Section Round Bloom, Arc Continuous Caster

摘要: Φ1 200 mm S355NL/Q355NE钢(Ceq 0.38~0.41)连铸圆坯的生产流程为100 t KR-BOF-LF-RH-R18 m连铸。采用全保护浇注、精确冷却工艺、三段式电磁搅拌、缓冷工艺等技术措施,过热度控制在15~45℃,拉速为0.14~0.20 m/min,电磁搅拌300 A/2 Hz,二冷比水量0.20 L/kg,圆坯入坑缓冷时间≥72 h,出坑温度≤300℃。检测结果表明,[O]≤0.001 8%、[H]≤0.000 08%;铸坯中心疏松≤1.5级、中心裂纹≤1.5级、缩孔≤0.5级;全截面碳含量极差≤0.07%;圆坯成分、低倍、表面均满足标准要求。圆坯经用户锻造成壁厚450~550 mm的风电法兰后,夹杂物、力学性能、内部探伤等质量指标检测结果,完全符合技术规范及用户使用要求。

关键词: Φ1 200 mm, 大截面连铸圆坯, 弧形连铸机