Behavior of Static Recrystallization of 0.75C-0.11V Microalloy Steel
Ren Anchao, Ji Yu, Zhao Longqi, Yuan Zexi, Song Xinli and Shen Dongdong
Special Steel . 2008, (2): 26 -27 .