Effect of Nb Content on Structure and Mechanical Properties of High Speed Steel W3Mo2Cr4V(Nb)
Zhang Yong, Ma Dangshen, Liu Jianhua, Chen Zaizhi, Yong Qilong
Special Steel . 2007, (3): 44 -46 .