ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

V-N Microalloyed Modified Containing Tungsten Cr5W Steel for Cold Rolling Working Roll
Wu Jianping , Jia Jianping , Wang Zidong
Special Steel . 2007, (5): 40 -41 .