ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Influence of Electromagnetic Brake on Impact to Solidified Shell and Temperature at Meniscus in CSP Mould
Xu Kuiri, Liu Guangmu, Meng Zhengbing, Yin Yanbo
Special Steel . 2006, (1): 11 -14 .