Grain Refinement Mechanism of 00Cr19Ni10 Austenite by Hot Equal Channel Angular Pressing
Wang Chang, Yang Gang, Wang Limin, Gao Yongliang , Zhong Hailin
Special Steel . 2007, (2): 10 -12 .