Structure and Mechanical Properties of Linepipe Steel X80
Zhang Xiaoli, Feng Yaorong, Zhao Wenzhen, Huo Chunyong, Zhuang Chuanjing, Ji Lingkang, Meng Qiang
Special Steel . 2006, (3): 11 -13 .