ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Numerical Simulation of Temperature Field of Mould Copper Plate for Slab Continuous Casting
Feng Ke, Xu Chushao, Chen Dengfu , Chen Guangbi
Special Steel . 2005, (1): 12 -15 .