Process Practice of Hot Forging Microalloying Steel F40MnV by Converter
Dai Guanwen, Liang Mei, Wu Yunfeng, Liu Xianming, Mao Tianrong, Chen Siliar, Wang Xinhu
Special Steel . 2005, (3): 57 -58 .