Effect of Swirling Flow Submerged Entry Nozzle on Quality of  Φ690 mm Continuous Casting Bloom of LZ50 Axle Steel
Zhao Zhigang, Zhang Jinwen, Wang Songwei, Wang Yutian
Special Steel . 2021, (1): 38 -42 .