Simulation of Material and Heat Balance of 150 t AOD Melting 430 Stainless Steel under Different Charge Conditions
Lu Xiaohui, Kang Congpeng, Chen Hongzhi, Xu Yongbin
Special Steel . 2025, (1): 134 -141 .  DOI: 10.20057/j.1003-8620.2024-00175