Influencing Factors and Process Control of Vacuum Consumable Remelting Arc Stability
Liu Wenxue, Liu Guanghui, Li Linsen, Fei Sanlin, XuYong, XieWei, Xu Guangpeng, Ni Yanhong
Special Steel . 2025, (3): 12 -17 .  DOI: 10.20057/j.1003-8620.2025-00065