ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Development and Production of C70S6BY Steel for Automobile  Engine Connecting Rod
Zhang Yuanpu, Wei Zehong, Zhang Huan, Bao Haiyan and Liang Baozhu
Special Steel . 2021, (6): 40 -42 .