赵丹婷, 刘爱强, 仇圣桃, et al. Physical and Mathematical Simulation on Flow Field of Liquid in 63t Tundish with a Filter[J]. Special Steel, 2016, 37(6): 22-26.DOI:
temperature field and inclusions moving trace in tundish for two strands slab casting with 3 kinds of structure-(a) turbulence inhibitor and wall + dam (original structure)
(b) turbulence inhibitor
wall + dam and channel filter and (c) turbulence inhibitor
wall and channel filter has been carried out by using geometric similarity 0. 29 : 1 water model and mathematical model. Results show that in tundish with original structure (a) the plug flow area is relatively small and the dead area is rather large; by adding channel liquid filter (b) the short circuit flow basically disappears
the dead volume in tundish decreases by 6. 83% and the average resident time of liquid increases from 287. 04 s to 373. 76 s
it is available to remove the inclusions from liquid and the effect of filter on drop in temperature of liquid is not obvious ; by using the filter to replace the dam (c) the effect of optimization is particularly obvious
that is the average residence time of liquid in tundish increases from 287. 04 s to 404.26 s
the peak time increases from original 95. 4 s to 190.8 s and the dead volume decreases from 36.10% to 8.76% .