[1] |
Zhai Wanli, Zhang Hongcai, Xiao Mengxuan, Xu Zhengzhou.
Control Technology of Aluminum Content and Inclusion Composition in High-silicon and Aluminum-controlled Steel
[J]. Special Steel, 2025, 46(2): 67-71.
|
[2] |
Li Haozhe, Jin Jinwen, Gao Fang, Gu Chao, Bao Yanpin, Wei Ze.
Research on the Metallurgical Properties of Fluorine-Containing Refining Slag and Its Fluoride-Free Design
[J]. Special Steel, 2025, 46(2): 72-77.
|
[3] |
Duan Fuchun, Wang Yuping, Zhu Zhiqiang.
Optimization of Electromagnetic Parameters for the 3rd-generation FC MOLD
[J]. Special Steel, 2025, 46(1): 126-133.
|
[4] |
Li Weitao, Wu Fapu, Yu Guangfu, Wang Huajun, Wang Kaimin, Jia Xingyu, Tang Haiyan.
Characteristics and Evolution of Non-metallic Inclusions in Metallurgical Production of GCr15 Bearing Steel
[J]. Special Steel, 2025, 46(1): 79-86.
|
[5] |
Ni Zhuowen, Zhu Hongchun, Li Huabing, Jiang Zhouhua, Sun Zhengxin, He Zhiyu.
Analysis of the Types and Distribution of Inclusions in H13 Die Steel Electroslag Ingots
[J]. Special Steel, 2024, 45(6): 48-52.
|
[6] |
Wang Li, Liu Chengbao, Li Haoqiu, Wang Yi, Sun Zonghui, Liu Chunwei, Yang Chaoyun, Fu Zhihao.
Effect of Rare Earth on Inclusions and Fatigue Properties of 20CrMnTi Gear Steel
[J]. Special Steel, 2024, 45(6): 117-124.
|
[7] |
Xie Kang, Mo Jinqiang, Zhang Wei, Wang Lijun.
The Effect and Control of Rare Earth Ce on Carbonitrides Precipitation in 441 Ferritic Stainless Steel
[J]. Special Steel, 2024, 45(6): 1-7.
|
[8] |
Yang Jianhua, Ju Yinjun, Yang Jun.
The Evolution Analysis and Removal of Oxide Inclusion in Tire Cord Steel XLX72 A
[J]. Special Steel, 2024, 45(5): 66-71.
|
[9] |
Liu Yong, Zhang Yunfei, Zhao YingLi, Zhao Nan, Zhao Zhengrong, Fan Mingqiang, Tian Zhiqiang.
Smelting Process Practice to Improve the Cleanliness and Polishling Proptice of Die Steel
[J]. Special Steel, 2024, 45(5): 47-52.
|
[10] |
Ren Ji, Yan Yun, Tian Jialong, Wang Lichao, Jiang Chenggang, Wang Lin, Jiang Zhouhua.
Effect of La Treatment on Inclusions in H13 Hot Work Die Steel
[J]. Special Steel, 2024, 45(4): 117-123.
|
[11] |
Gao Xiaoyong, Zhang Lifeng.
Effect of Electroslag Remelting Using 37 Slag on Inclusions in M50 High-temperature Bearing Steel
[J]. Special Steel, 2024, 45(4): 89-93.
|
[12] |
Liu Ye, Gui Yulin, Yin Qing, Wu Xiaolin, Miao Xinde.
Research on Ultra-high Rotary Bending Fatigue Strength of Flexible Bearing Steels for Robot Harmonic Speed Reducer
[J]. Special Steel, 2024, 45(3): 105-113.
|
[13] |
Chen Yufeng, Zhang Junfen, Xue Qihe, Bai Jun, Yang Shufeng, Li Jingshe.
Effect of Nitrogen Content and Final Rolling Temperature on
Low- temperature Impact Toughness of Titanium
Microalloyed High- strength Steel CGLC700
[J]. Special Steel, 2024, 45(3): 40-18.
|
[14] |
Pan Hujiang, Yang Xinming, Li Guangqiang, Yang Zhizheng, Huo Xudong.
Effect of Ti Microalloying on the Structure and Properties of High Manganese Steel
[J]. Special Steel, 2024, 45(2): 74-78.
|
[15] |
Jiang Yaqing, Chen Jun, Huang Chenggang, Li Bo, Li Qian, Jiang Yanfeng.
Effect of Tundish Coating on Cleanliness of GCr15 Bearing Steel
[J]. Special Steel, 2024, 45(1): 61-64.
|