ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2005, Vol. 26 ›› Issue (4): 13-15.

Previous Articles     Next Articles

Dynamic Recrystallization Behavior of Steel B30MnSi

Wei liqun   

  1. Material Engineering Department, Shanghai Institute of Technology, Shanghai 200235 
  • Received:2005-01-20 Online:2005-08-01 Published:2023-04-08

B30MnSi钢的动态再结晶行为

魏立群   

  1. 上海应用技术学院材料工程系,上海200235
  • 作者简介:魏立群(1962-),男,副教授。1983年上海工业大学毕业, 从事轧制工艺研究
  • 基金资助:
    上海市教委科学技术基金重点项目(03ZH01)

Abstract: The compression deformation test at temperature between 850 T and 1 000 X. with strain rate 0.1 * 10 1/s of steel BSOMnSi- 0.32C, 1.04Mn, 0.85Si, 0.019P, 0.009S has been carried out using Gleeble-1500 thermal simulation machine to study the dynamic recrystallization behavior of the steel. And the relation of peak stress σm , peak strain % , dynamic recrystallization critical strain q with temperature compensating deformation rate factor Z has been got by regression analysis, that is am = 16.689Ln(Z) - 347.41, Ep = 0.047 4Ln(Z) - 1.102 3, and e^. «s0.039 3Ln(Z) - 0.915.

Key words:  , Steel B30MnSi, Rod, Stress- Strain, Dynamic Recrystallization

摘要: 采用Gleeble1500热模拟试验机对B30MnSi钢(%:0.32C,1.04Mn,0.85Si,0.019P,0.009S)进行变形温度为850~1000℃,应变速度为0.1~101/s的压缩变形试验,以研究该钢的动态再结晶规律。并通过回归分析得出峰值应力σm,应变εp,动态再结晶临界应变εc与温度补偿变形速率因子Z之间关系式为σm=16.689Ln(Z)-347.41;εp=0.0474Ln(Z)-1.1023;εc≈0.0393Ln(Z)-0.915。

关键词: B30MnSi钢,线材, 应力-应变,动态再结晶