Zener-Hollomon Equation of a Ti-IF Steel Deformed at 750 ~ 850℃

Xu Guang, Xu Chushao   

  1. College of Material Science and Engineering, Chongqing University, Chongqing 400044
  • Received:2005-07-07 Online:2006-10-01 Published:2006-10-01

Ti-IF钢750 ~ 850℃变形的Zener-Hollomon 参数方程

徐光, 徐楚韶   

  1. 重庆大学材料科学与工程学院,重庆400044
  • 作者简介:徐光(1961-),男,教授,系副主任,从事金属材料加工 工艺和组织性能控制研究
  • 基金资助:
    湖北省教育厅重点科研项目(2002A01010)

Abstract: The single pass reduction deformation experiments of a Ti-IF steel (0. 009C, 0. 047Ti) at 750 ~ 850 °C with strain rate of deformation 1 -70 s-1 have been carried out by THERMECMASTOR-Z thermal simulation machine. Based on obtained stress - strain curves with different temperature and strain rate of deformation, it showed that with increasing speed and strain of deformation, the flowing stress increased, while at experimental temperature range the effect of deformation temperature on flowing stress was not obvious. The relation between Zener-Hollomon parameter Z of the Ti-IF steel and strain rate e and temperature T of deformation was Z = ε exp(42 150/T)

Key words: Ti-IF Steel, Deformation at 750 - 850 °C, Zener-Hollomon Equation

摘要: 通过THERMECMASTOR-Z热模拟机对成分(% )为0. 009C.0. 047Ti ,的Ti-IF钢进行750 ~ 850 ℃变形速率1 ~ 70 s-1的单道次压缩变形试验。从不同变形温度和速度下所得应力-应变曲线表明,随变形速 率和应变的增加,流动应力增大,但在实验温度范围内,变形温度对流动应力的影响不显著。该Ti-IF钢的 Zener-HoHomon参数Z与变形速率b和变形温度T的关系为:Z = ε exp(42 150/T)