Mathematical Modeling and Application of Controlled Cooling Line of High-Speed Rolling Rod 82B

Xu Jinqiao, Liu Yazheng, Zhou Shumei   

  1. School of Materials Science and Engineering, University of Science and Technology, Beijing 100083
  • Received:2006-03-06 Online:2006-10-01 Published:2006-10-01

高速线材82B控制冷却线的数学模型和应用

徐进桥,  刘雅政,  周淑梅   

  1. 北京科技大学材料科学与工程学院,北京100083

Abstract: The mathematical modeling of finished Φ12. 5 mm rod temperature at water cooling zone and blast cooling zone of 62.7 m controlled cooling line for rod 82B (0. 80 -0. 82C, 0. 6 -0. 9Mn, 0. 016V) has been studied by using commercial FEM software Marc. The comparison between model calculated results and measured results at situ showed that the error was<25℃

摘要: 釆用商用有限元软件Marc,模拟研究了成分(% )为0. 80 -0. 82C,0.6-0. 9Mn,0.016V成品规 格Φ12. 5 mm高速线材82B的62.7 m控制冷却线水冷段和风冷段过程的钢材温度的数学模型。模拟计算的 结果与现场实测值对比表明,其误差<25℃