Abstract: The experiment on calcined denitriding process of recarburizer 95(containing 0. 10%N),petroleum coke(0.93%N)and pitch coke(0.40% N)has been carried out. The results indicated that with increasing cal- cined temperature the nitrogen content in 3 kinds of recarburizer decreased and as the temperature was more than 2000℃,the nitrogen content in each recarburizer was less than 100×10-6.As calcined temperature was 1800℃, the nitrogen content in recarburizer 95 was less than 300×10-6 while that in petroleum coke or pitch coke was less than 100×10-6.
摘要: 对95增碳剂(0.10%N)、石油焦(0.93%N)和沥青焦(0.40%N)进行煅烧脱氮试验,试验结果 表明:随煅烧温度的提高,3种增碳剂中的氮含量都下降,温度大于2000 ℃时,各增碳剂中的氮含量均小于 100×10-6 。1800℃煅烧时,95增碳剂的氮含量小于300×10-6,石油焦或沥青焦的氮含量小于100×10-6。
Sun Yaqin, Chen Qizhong, Zhang Zhuo and Jin Minglin. Experiment on Calcined Denitriding Process of Recarburizer[J]. Special Steel, 2006, 27(5): 30-31.
孙亚琴, 陈麒忠, 张 琢, 金鸣林. 增碳剂煅烧脱氮工艺实验研究[J]. 特殊钢, 2006, 27(5): 30-31.
Add to citation manager EndNote|Ris|BibTeX
URL: https://www.specialsteeljournal.com/EN/
https://www.specialsteeljournal.com/EN/Y2006/V27/I5/30