ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2006, Vol. 27 ›› Issue (5): 43-45.

Previous Articles     Next Articles

Development of φ140 mm Round Bar for R4 Offshore Mooring Chain

Qian Gang¹²,Lei Yinghua²,Chen Changxi²,Zheng Wenchao², Chen Jun²   

  1. 1 School of Metallurgy and Ecological Engineering,University of Science and Technology,Beijing 100083;
    2 Daye Special Steel Corp Ltd,Huangshi 435001
  • Received:2006-05-10 Online:2006-10-01 Published:2023-04-20

R4 级海洋系泊链φ140 mm 圆钢的开发

钱  刚1.2 雷应华2 陈长西2 郑文超2  陈  君2   

  1. 1北京科技大学冶金与生态工程学院,北京100083;
    2大冶特殊钢股份有限公司,黄石435001
  • 作者简介:钱刚(1966-),男,高级工程师,《特殊钢》编委会副主任委员,上海大学毕业,从事特殊钢冶金和工艺研究。

Abstract: The φ140 mm of steel(0.21C,1.45Mn,1.44Cr,1.21Ni,0.49Mo,0.07Nb)for R4 of fshore mooring chain was produced at Daye  Steel by 60 t EBT are fumnace -70 t LF refining + RH vacuum degassing -3 strand 350mm×470 mm billet caster -850 primary mill blooming -750 semi-continuous mill rolling process. The re-  sults showed that with LF refining for 45 min,feeding Al wire and Ca-Si wire deoxidizing,then ≤66.65 Pa RH vacuum degassing for 20min + soft argon blowing for ≥10 min,the oxygen content in finished products of steel for off shore mooring chain was 14.8×10-6,nitrogen content 69.8×10-6,hydrogen content 1.2×10-6,segregation porosity rating were 0.5,inclnsion rating 0~1, impact energy at -40 ℃≥100 and each index met the require ment of standard.

摘要: 大冶特钢采用60tEBT 电弧炉-70 tLF 精炼+RH 脱气-3流350mm×470 mm方坯连铸机-850 mm 初轧+750mm 半连轧工艺生产了成分(%)为0.21C、1.45Mn、1.44Cr、1.21Ni、0.49Mo、0.07Nb φ140 mm R4 级系泊链钢。结果表明,通过LF 精炼45 min,喂Al线和Ca-Si线脱氧后,进行RH≤66.65 Pa真空处理20 min+ 软吹氩≥10min,使系泊链钢成品中的氧含量达14.8×10-6,氮含量69.8×10-6,氢含量1.2×10-6,偏 析和疏松0.5级,夹杂物0~1级, -40℃时冲击功≥100J,各类指标均满足标准要求。