Coupled Numerical Simulation of Flow Field and Temperature Field in Slab Concasting Filling Process

Jin Yanjuan1, Cui Xiaochao1, Li Lang1, Zhang Zhu1, Liu Cai2   

  1. 1 School of Application Science, Taiyuan University of Science and Technology, Taiyuan 030024 ;
    2 Hebei Academy of Sciences, Shijiazhuang 050081
  • Received:2006-03-22 Online:2006-10-01 Published:2006-10-01

板坯连铸充型过程流场温度场耦合数值模拟

晋艳娟1, 崔小朝1, 李朗1, 张柱1, 刘才2   

  1. 1太原科技大学应用科学学院,太原030024;
    2河北省科学院,石家庄050081
  • 作者简介:晋艳娟(1979-),女,硕士研究生,液态金属流动多场耦合 数值模拟研究
  • 基金资助:
    国家自然科学基金资助项目(编号50474013)
    河北省科技攻关项目(编号05242226d)

Abstract: The flow and solidification status of molten steel with coupling flow field and temperature field in inner- outer couple cooling mold has been simulated by using CFD commercial code Flow-3 d software to get distributing diagrams of flow field and temperature, and free-surface level and shape diagram. The influence of flow field and temperature field in slab concasting filling process on solidification of molten steel was analyzed. It is indicated that the inner cooler could improve the molten steel flow status which is favourable for inclusion floating up in molten steel and increasing the solidification rate of molten steel

摘要: 利用CFD商用软件Flow-3d,对内外复合冷却结晶器内钢水充型过程流场温度场耦合作用下的 流动和凝固状况进行数值模拟,得到了流场温度场的分布图和充填过程中自由表面的位置和形状图。分析了 板坯连铸充型过程中流场温度场对钢水凝固的影响。结果表明内冷却器可改善钢水的流动,有利于钢液中的 夹杂物上浮,加快结晶器内钢液的凝固