Effect of Long Nozzle Casting with Shielding Argon Gas on Quality of Φ450 mm Round Billet of Wheel Steel
Wu Zongshuang1, Bao Yanping1, Liu Jianhua1, Chen Gang2, Gong Zhixiang2, Zhong Bin2
1 School of Metallurgical and Ecological Engineering, University of Science and Technology, Beijing 100083;
2 Maanshan Iron and Steel Co Ltd, Maanshan 243002
Wu Zongshuang, Bao Yanping, Liu Jianhua, Chen Gang, Gong Zhixiang, Zhong Bin. Effect of Long Nozzle Casting with Shielding Argon Gas on Quality of Φ450 mm Round Billet of Wheel Steel[J]. Special Steel, 2007, 28(2): 54-55.
1 Hudd,R C.Some Aspects of the Annealing of Low Carbon Strip Steel. Metals and Materials,1987,3(2):71
2 Morison W B,Nitrogen in the Steel Product. Ironmaking and Steelmaking,1989,16(2):12
3 康大韬.大型锻件材料及热处理.北京:龙门书局出版社,1998