ISSN:1003-8620

CN:42-1243/TF

Governed by: CITIC Pacific Special Steel Group Co., LTD

Sponsored by: Daye Special Steel Co., LTD.

Special Steel ›› 2007, Vol. 28 ›› Issue (3): 28-29.

Previous Articles     Next Articles

Mechanical and Magnetic Properties of Cold Rolled 0.02C-6.56Si High Silicon Steel Sheet

Liu  Yan,Liang  Yongfeng,Ye  Feng,Lin  Junpin  ,Chen  Guoliang   

  1. State Key Laboratory for Advanced Metals and Materials,University of Science and Technology,Beijing 100083
  • Received:2006-11-21 Online:2007-05-01 Published:2023-01-31

冷轧0.02C-6.56Si高硅钢薄板的力学和磁性能

刘艳,梁永锋,叶丰,林均品,陈国良   

  1. 北京科技大学新金属材料国家重点实验室,北京100083
  • 作者简介:刘 艳(1982-),女,硕士,高硅钢薄板的轧制及其磁性能研究 。
  • 基金资助:
    “973”国家重点基础研究发展计划(2006CB605205- 2)和“北京科技大学422高层次创新人才工程 (00007425)”基金联合资助项目。

Abstract: The manufacture process of sheet of  high silicon steel  0.02C,6.56Si,0. 14Mn,0.013P,0.004S, 0.02Al was melting by 25  kg  vacuum  induction  furnace,  forging  breakdown,hot  rolling  to  1mm  at  1050~850  ℃,warm rolling  to 0.3  mm  at  650℃,and  cold  rolling  to 0.05  mm.The  non-oriented  silicon  steel  was  got  by  vacuum  annealing  of the  cold rolled  sheet  at  1200  ℃ for1.5 h.  Compared with  conventional  oriented  silicon  steel,the  iron  loss  of high  silicon steel  sheet  decreased  by  14.7%  with0.07  Tand  20  kHz,  by  19.7%  with  30  kHzand  by  28. 1%  with  40  kHz,it  is  an  excellent soft magnetic material.  The tensile  strength  of the  steel  sheet  cold rolled was up to 1480 MPa.

Key words: High Silicon Steel,Cold Rolling,Magnetic Property

摘要: 通过25 kg真空感应炉熔炼,锻造开坯,1050~850℃热轧至1 mm,650℃温轧至0.3 mm,再冷轧成0.05 mm高硅钢(%:0.02C、6.56Si、0.14Mn、0.013P、0.004S、0.02Al)薄板。冷轧板经过1 200℃1.5 h真空退火后,得到无取向硅钢。与普通取向硅钢相比,在0.07 T,20 kHz的高硅钢薄板铁损降低14.7%,30 kHz的铁损降低19.7%,40 kHz的铁损降低28.1%;该钢是一种优良的软磁材料,在冷轧后的强度达1 480 MPa。