Effect of Deforming Temperature on Structure and Precipitates of 0.05C-0.13Nb Steel

Wen  Jianhua1,2,Sun  Xinjun2,Liu  Qingyou2,Yin Shubiao2,Xiang  Jinzhong1   

  1. 1  School  of Physical  Science  and  Technology,Yunnan  University,Kunming  650091;
    2  Institute  for  Structural  Materials,Center  Iron  and  Research  Institute,Beijing  100081
  • Received:2006-12-05 Online:2007-05-01 Published:2023-02-01

变形温度对0.05C-0.13Nb钢组织和析出物的影响

文建华1,2,孙新军2,刘清友2,阴树标2,项金钟1   

  1. 1 云南大学物理科学技术学院,昆明650091;
    2钢铁研究总院结构材料研究所,北京100081
  • 作者简介:文建华(1982-),男,2004年云南大学毕业,从事低合金钢等材料研究。

Abstract: The structure and precipitates of 0.05C-0. 13Nb steel deformed by 50% at different temperature between 950~750  ℃ have been  studied by  Gleeble- 1500D thermal  simulation machine,SEM  and  TEM. Results  showed that with  deforming  temperature  decreasing  from  950  ℃  to750  ℃,the  polygonal  ferite  content(volume  percent)in  0.05C-0. 13Nb  steel increased from 20% to 80% and grain size of polygonal ferrite decreased from 9 μm to4 μm; the deformed structure  in  steel  consisted  of polygonal  ferite,grain bainite  and  1~3 μm martensite/austenite  island;  and the  amount  of 1~10 nm
precipitates Nb (C,N) in steel increased with decreasing deformed temperature.

Key words: Deforming Temperature, 0.13Nb Steel, Structure, Precipitates

摘要: 用Gleeble-1500D热模拟试验机和电子显微镜研究了在950~750℃不同温度下变形50%后0.05C- 0.13Nb钢的组织和析出相。结果表明,随变形温度由950℃下降至750℃,0.05C-0.13Nb钢中多边形铁索体含量(体积分数)由20%增至80%,多边形铁素体晶粒尺寸由9μm降至4μm;变形后的组织由多边形铁索体、粒状贝氏体和1~3μm马氏体/奥氏体岛组成;钢中的析出物为1~10 nm的Nb(C,N),随变形温度降低析出物数量增加。

关键词: 变形温度, 0.13Nb钢, 组织, 析出物