Effect of LF(VD)Refining Process on Control of Sulphur and Sulphide in Gear Steel 28MnCr5

Li  Guozhong1,2,Wang  Fuming1,Cao  Hongfu2   

  1. 1 Metallurgical and Ecological Engineering,University of Science and Technology,Beijing 100083;
    2 Jiangyin Xingcheng Special Steel Co Ltd,Jiangyin 214429
  • Received:2006-12-25 Online:2007-05-01 Published:2023-02-03

LF(VD)精炼工艺对控制28MnCr5齿轮钢中硫和硫化物的影响

李国忠1,2,王福明1,曹红福2   

  1. 1北京科技大学冶金与生态工程学院,北京100083;
    2江阴兴澄特种钢铁有限公司,江阴214429
  • 作者简介:李国忠(1967-),男,高级工程师,《特殊钢》编委。

Abstract: The basicity of refining slag,feeding sulphur wire and deoxidation process for a 45 t LF on control of sulphur,oxide content    and sulphide in steel 28MnCr5(0.25~0.30C,0.60~0.80Mn,0.020~0.035S,0.80~1.00Cr)  have been tested. Results showed that as feeding sulphur wire with basicity of LF refining slag-2.8~5. 1,the yield of sulphur after VD was up to 80%~90% and oxide rating in steel≤1.5;and feeding suitable amount of CaSi wire was available to improve the morphology of sulphide in steel.

Key words: 45 t LF,Refining Process,Gear Steel 28MnCr5,Sulphide

摘要: 试验了45 t LF精炼渣的碱度、喂硫线和脱氧工艺对28MnCr5钢(%:0.25~0.30C、0.60~0.80Mn、0.020~0.035S、0.80~1.00Cr)硫含量的控制、氧化物含量和钢中硫化物的影响。结果表明,LF精炼渣碱度控制在2.8~5.1喂硫线,VD后硫的回收率达80%~90%;钢中氧化物级别≤1.5级;精炼结束喂适量CaSi线可改善钢中硫化物的形貌。

关键词: 45tLF, 精炼工艺, 28MnCr5齿轮钢, 硫化物